Saturday, October 4, 2008

Torch Soldering vs. Soldering Iron

There are several posts on my blog regarding making soldered glass slide and pebble jewelry. That application calls for using a soldering iron, like those used for connecting pieces of stained glass. The basic elements of that method of soldering apply to torch soldering as well.... metal-to-metal contact, the use of flux to flow the solder, the use of solder & a heating tool that reaches the temperature that is necessary to melt the solder. But the methods are not necessarily interchangeable. For example, you cannot use torch soldering to make the glass slide pendants. The heated area is too broad and too hot. The copper tape & paper artwork would melt and the glass would shatter. But the torch method is the best choice for heat connecting precious metals like silver. A soldering iron tip must be touching the solder to melt it and therefore, it would get in the way when trying to make the small unnoticeable connections that are desired for finer jewelry, whereas the torch only needs to be in proximity to the area of connection to form a heat source that will melt the solder and draw the molten liquid to it. The torch is hot enough to melt solder with a higher precious metal content than the soldering iron generally, so for that reason it is preferred for fine jewelry as well.

There are a few pre and post solder steps that are required when torch soldering silver. When silver (other than pure fine silver or argentium silver) is exposed to high heat, it gets something that is called "Fire Scale" which totally discolors the silver and it is very difficult to remove because it goes deep into the metal. This happens because of the copper content that is alloyed in sterling silver. For this reason, I work with fine silver only, but sometimes the strength of sterling is necessary.

To avoid fire scale, you can prepare the pieces of silver by soaking them in a prep solution designed specifically to address fire scale. Also, some people lay the silver on a chunk of natural charcoal (not BBQ charcoal!) when soldering to help absorb oxygen which is in part to blame for fire scale.

I found this information in the Art Jewelry Mag forum by "bleugurl" but I have not personally verified it:
"To prevent fire scale, stop oxygen from getting in contact with the metal. Fire scale is formed whenever silver and sterling is heated above about 1000 degrees F. Oxygen combines with copper to form cuprous oxide which exhibits as firescale.

Prips Flux, denatured alcohol/borax solution, Cupronil…any of these products will work. You might try coating the whole piece in flux before soldering. Be generous with the flux. To properly apply anti-firescale-fluxes, the metal must be heated slightly. Paint, dip the piece or spray on the anti-fs-flux. A mist atomizer bottle works well here. If the metal temperature is correct a white grainy coating will form. Quickly play a flame across the wet fluxed metal to dry it. This will evaporate the alcohol, leaving a white coating of tiny borax crystals."

After soldering, the piece must be pickled to clean all of the residue and flux from it.

This video created by http://www.cooltools.us/ demonstrates how to coat your pieces with prep solution and some handy tricks for soldering small parts like jump rings with a torch. Check it out. I hope it helps you as much as it helped me.



Here is another video demonstrating another method for coating with flux & torch soldering on a piece of charcoal:




Happy soldering!

Wednesday, August 6, 2008

An "Oops" Turned Around - Rescuing Precious Metal Clay from Boo Boos at Any Stage

Funny story... the brown stone you see here is actually blue tanzanite. I made this pure silver pendant with a blue stone and the words "blue moon" stamped at the bottom. However, the stone is more heat sensitive than I realized...when I fired it in the kiln, it turned brown. Luckily it is a gorgeous brown stone with red & gold fire (the picture does not do it justice), but it was obviously out of place with the words "blue moon", so I thought hard about how I could salvage this pendant that I really liked and came up with the idea to cover "blue moon" with "eclipse' because the moon looks brown during an eclipse, right? So the pendant ended up being something completely different than I planned, and the "oops" turned into something that is kinda cool and different I think.

So far there is nothing that I have done with metal clay that has not been salvagable no matter how hard I try to screw it up!

Before the clay is fired...
  • In the wet stage, you can always ball it up and start over or augment with more clay.
  • If the clay starts to get dry before you are done forming, spritz with water.
  • In the dry greenware state it can be turned right back into clay by spritzing generously with water and sealing in plastic or an airtight container for a day or so.
  • If at any time you make it too wet, expose to the air until it is the right consistancy.
  • If you break a piece in the leatherhard or greenware state, you can use the metal clay paste to glue things back together.
  • You can refine edges and smooth flaws with a wet paintbrush or with sand paper. (If you sand the greenware, be sure to salvage the 'dust' from you sanding and add it to your paste jar. The moisture will turn the dust into more paste or slip so there is no waste.)
  • If cracks form while drying, you can 'spackle' them with silver paste.

After the clay is fired...

  • You can repair breaks using silver OIL paste and re-fire (Kiln only), then sand and polish until the seam is not visible.
  • You can add another element made from metal clay and use paste to adhere it to the original piece then refire.
  • You can enamel, paint, or collage over mistakes (as I did in the eclipse pendant) to turn the item into a mixed media piece.
  • You can file off small mistakes using metal files and different grits of sand paper or if you have metalsmithing tools, you can saw off boo boos or drill, etc.
  • If all else fails, the item is .999 silver and can be melted and poured into a mold or can be sold to a precious metal buyer for the going rate for pure silver.

I just love a hobby with built in safety net!!